Development of 25- \mu{\rm m} -Pitch Microbumps for 3-D Chip Stacking

Sign In

Cookies must be enabled to login.After enabling cookies , please use refresh or reload or ctrl+f5 on the browser for the login options.

Formats Non-Member Member
$31 $13
Learn how you can qualify for the best price for this item!
Become an IEEE Member or Subscribe to
IEEE Xplore for exclusive pricing!
close button

puzzle piece

IEEE membership options for an individual and IEEE Xplore subscriptions for an organization offer the most affordable access to essential journal articles, conference papers, standards, eBooks, and eLearning courses.

Learn more about:

IEEE membership

IEEE Xplore subscriptions

17 Author(s)
Aibin Yu ; Inst. of Microelectron., Agency for Sci., Singapore, Singapore ; Kumar, A. ; Soon Wee Ho ; Hnin Wai Yin
more authors

The development of ultrafine-pitch microbumps and the thermal compression bonding (TCB) process for advanced 3-D stacking technology are discussed in this paper. Microbumps, consisting of Cu pillars and thin Sn caps with a pitch of 25 μm, are fabricated on an Si chip by the electroplating method. Total thickness of the Cu pillar and the Sn cap is 10 μm. Electroless nickel and immersion gold pads with a total thickness of 4 μm are fabricated on an Si carrier. TCB of the Si chip and the Si carrier is conducted on an FC150 flip-chip bonder, and a good joining with higher than 10-MPa die shear strength is achieved. After bonding, the bond line thickness between the Si chip and the Si carrier is filled with the selected capillary underfill material. Void-free underfilling is achieved with underfill materials which have a fine filler size. Ninety percent of the bonded samples can pass the thermal cycling test (-40/+125°C) with 1000 cycles and the highly accelerated temperature/humidity stress test (130°C , 85% RH) for 96 h.

Published in:

Components, Packaging and Manufacturing Technology, IEEE Transactions on  (Volume:2 ,  Issue: 11 )