Fabrication of multilayer systems combining microfluidic and microoptical elements for fluorescence detection

Sign In

Cookies must be enabled to login.After enabling cookies , please use refresh or reload or ctrl+f5 on the browser for the login options.

Formats Non-Member Member
$31 $13
Learn how you can qualify for the best price for this item!
Become an IEEE Member or Subscribe to
IEEE Xplore for exclusive pricing!
close button

puzzle piece

IEEE membership options for an individual and IEEE Xplore subscriptions for an organization offer the most affordable access to essential journal articles, conference papers, standards, eBooks, and eLearning courses.

Learn more about:

IEEE membership

IEEE Xplore subscriptions

6 Author(s)
Roulet, J.-C. ; Inst. of Microtechnology, Neuchatel Univ., Switzerland ; Volkel, R. ; Herzig, Hans-Peter ; Verpoorte, E.
more authors

This paper presents the fabrication of a microchemical chip for the detection of fluorescence species in microfluidics. The microfluidic network is wet-etched in a Borofloat 33 (Pyrex) glass wafer and sealed by means of a second wafer. Unlike other similar chemical systems, the detection system is realized with the help of microfabrication techniques and directly deposited on both sides of the microchemical chip. The detection system is composed of the combination of refractive microlens arrays and chromium aperture arrays. The microfluidic channels are 60 μm wide and 25 μm deep. The utilization of elliptical microlens arrays to reduce aberration effects and the integration of an intermediate (between the two bonded wafers) aluminum aperture array are also presented. The elliptical microlenses have a major axis of 400 μm and a minor axis of 350 μm. The circular microlens diameters range from 280 to 300 μm. The apertures deposited on the outer chip surfaces are etched in a 3000-Å-thick chromium layer, whereas the intermediate aperture layer is etched in a 1000-Å-thick aluminum layer. The overall thickness of this microchemical system is less than 1.6 mm. The wet-etching process and new bonding procedures are discussed. Moreover, we present the successful detection of a 10-nM Cy5 solution with a signal-to-noise ratio (SNR) of 21 dB by means of this system

Published in:

Microelectromechanical Systems, Journal of  (Volume:10 ,  Issue: 4 )