Cart (Loading....) | Create Account
Close category search window
 

Surface hydrogen incorporation and profile broadening caused by sheath expansion in hydrogen plasma immersion ion implantation

Sign In

Cookies must be enabled to login.After enabling cookies , please use refresh or reload or ctrl+f5 on the browser for the login options.

Formats Non-Member Member
$31 $13
Learn how you can qualify for the best price for this item!
Become an IEEE Member or Subscribe to
IEEE Xplore for exclusive pricing!
close button

puzzle piece

IEEE membership options for an individual and IEEE Xplore subscriptions for an organization offer the most affordable access to essential journal articles, conference papers, standards, eBooks, and eLearning courses.

Learn more about:

IEEE membership

IEEE Xplore subscriptions

4 Author(s)
Fan, Zhineng ; Dept. of Phys. & Mater. Sci., City Univ. of Hong Kong, Kowloon, China ; Zeng, Xuchu ; Tat-Kun Kwok, D. ; Chu, P.K.

Hydrogen plasma immersion ion implantation (PIII) in conjunction with ion-cut is an efficient and economical technique to synthesize silicon-on-insulator (SOI) substrates. Unlike beam-line ion implantation, the PIII hydrogen profile usually exhibits multiple peaks because of different implanted species, such as H+, H2 +, and H3+. In addition, a certain amount of adsorbed hydrogen exists near the surface and the hydrogen in-depth distribution is broader than that of a beam-line implant also as a result of a low-energy component. For the ion-cut process, the broadened hydrogen profile and surface hydrogen can decrease the efficiency of the blistering process, induce uneven exfoliation, and degrade the interfacial quality of the bonded wafer. Hydrogen can adsorb on the wafer surface during the “off-cycle” of the sample voltage pulse and consequently be driven in by ion mixing or diffusion. In order to reduce surface hydrogen incorporation, the implantation time must be short, and this requires an efficient cooling mechanism on the sample stage because a high ion current is needed to implant a high dose in a short time (less than 5 min). Another mechanism of profile broadening is that the expanding sheath creates low-energy ions during PIII. Our experimental and simulation data disclose that profile broadening is less severe for a shorter sample voltage pulsewidth and that good blistering characteristics can be achieved using a long pulse, in spite of a relatively long implantation time of 1 h

Published in:

Plasma Science, IEEE Transactions on  (Volume:28 ,  Issue: 2 )

Date of Publication:

Apr 2000

Need Help?


IEEE Advancing Technology for Humanity About IEEE Xplore | Contact | Help | Terms of Use | Nondiscrimination Policy | Site Map | Privacy & Opting Out of Cookies

A not-for-profit organization, IEEE is the world's largest professional association for the advancement of technology.
© Copyright 2014 IEEE - All rights reserved. Use of this web site signifies your agreement to the terms and conditions.