By Topic

Electrical and noise properties of thin-film transistors on very thin excimer laser annealed polycrystalline silicon films

Sign In

Cookies must be enabled to login.After enabling cookies , please use refresh or reload or ctrl+f5 on the browser for the login options.

Formats Non-Member Member
$31 $13
Learn how you can qualify for the best price for this item!
Become an IEEE Member or Subscribe to
IEEE Xplore for exclusive pricing!
close button

puzzle piece

IEEE membership options for an individual and IEEE Xplore subscriptions for an organization offer the most affordable access to essential journal articles, conference papers, standards, eBooks, and eLearning courses.

Learn more about:

IEEE membership

IEEE Xplore subscriptions

3 Author(s)
Dimitriadis, C.A. ; Dept. of Phys., Thessaloniki Univ., Greece ; Stoemenos, J. ; Kamarinos, G.

Thin-film transistors, fabricated on polycrystalline silicon films prepared by combined solid phase crystallization of amorphous silicon and excimer laser annealing processes, have been investigated by electrical and low frequency noise measurements in relation to the active layer thickness and the laser energy density. The device performance is improved with increasing the laser energy density until a critical value where the film is completely melted. By decreasing the active layer thickness from 50 to 25 nm, although the subthreshold characteristics are improved, the electron mobility and the threshold voltage are degraded. The noise data indicate that the degradation is related to electron trapping in both gate and substrate oxide interface traps