Mn-Zn ferrite with MoO3 and other oxide additives

Sign In

Cookies must be enabled to login.After enabling cookies , please use refresh or reload or ctrl+f5 on the browser for the login options.

Formats Non-Member Member
$31 $13
Learn how you can qualify for the best price for this item!
Become an IEEE Member or Subscribe to
IEEE Xplore for exclusive pricing!
close button

puzzle piece

IEEE membership options for an individual and IEEE Xplore subscriptions for an organization offer the most affordable access to essential journal articles, conference papers, standards, eBooks, and eLearning courses.

Learn more about:

IEEE membership

IEEE Xplore subscriptions

3 Author(s)
Ono, K. ; FDK Corp., Shizuoka, Japan ; Fukunaga, S. ; Matsuo, Y.

We studied the effects of mixing a high-permeability Mn-Zn ferrite with two different additives simultaneously-MoO3 (known to promote grain growth) and another oxide having a low melting point. We found that, paired with MoO3, V2O5 had an effect of speeding up ferrite shrinkage, thereby enabling the sintering of ferrites in a shorter time or at a lower temperature. Similarly coupled with MoO3, PbO had an effect of increasing the ferrite shrinkage rate, resulting in a higher permeability of the ferrite with an initial-permeability measurement of 25,500

Published in:

Magnetics, IEEE Transactions on  (Volume:35 ,  Issue: 5 )