By Topic

Misch metal-Fe-B melt spun magnets with 8 MGOe energy product

Sign In

Cookies must be enabled to login.After enabling cookies , please use refresh or reload or ctrl+f5 on the browser for the login options.

Formats Non-Member Member
$31 $13
Learn how you can qualify for the best price for this item!
Become an IEEE Member or Subscribe to
IEEE Xplore for exclusive pricing!
close button

puzzle piece

IEEE membership options for an individual and IEEE Xplore subscriptions for an organization offer the most affordable access to essential journal articles, conference papers, standards, eBooks, and eLearning courses.

Learn more about:

IEEE membership

IEEE Xplore subscriptions

8 Author(s)
Yamasaki, J. ; Kyushu Institute of Technology, Sensui-cho, Tobata, Kitakyushu, Japan ; Soeda, H. ; Yanagida, M. ; Mohri, K.
more authors

The magnetic and structural properties of melt spun MM-Fe-B ribbons, where MM stands for misch metal, were examined. It has been shown that the MM16Fe75B9ribbon can exhibit a coercive force of 9.4 kOe and an energy product of 8.1 MGOe when it was quenched at the optimum rate of 20 m/sec, in terms of quenching wheel surface velocity. Microstructural and X-ray analysis revealed that the optimum-quenched ribbons consist of grains with size from less than 10 nm to 300 nm, and have c-axis orientation in the free surface. The plastic magnets made of the optimum-quenched ribbons have been shown to exhibit a coercive force of 7.6 kOe and an energy product of 4.4 MGOe, which compare favorably to anisotropic ferrite magnets.