Cart (Loading....) | Create Account
Close category search window
 

Packaging of copper/low-k IC devices: a novel direct fine pitch gold wirebond ball interconnects onto copper/low-k terminal pads

Sign In

Cookies must be enabled to login.After enabling cookies , please use refresh or reload or ctrl+f5 on the browser for the login options.

Formats Non-Member Member
$31 $13
Learn how you can qualify for the best price for this item!
Become an IEEE Member or Subscribe to
IEEE Xplore for exclusive pricing!
close button

puzzle piece

IEEE membership options for an individual and IEEE Xplore subscriptions for an organization offer the most affordable access to essential journal articles, conference papers, standards, eBooks, and eLearning courses.

Learn more about:

IEEE membership

IEEE Xplore subscriptions

2 Author(s)
Chungpaiboonpatana, S. ; Dept. of Chem. Eng. & Material Sci., Univ. of California, Irvine, CA, USA ; Shi, F.G.

The trend toward finer pitch and higher performance devices has driven the semiconductor industry to incorporate copper and low-k dielectric materials. Compared to the commonly used aluminum metallization scheme on the traditional silicon dioxide and/or silicon nitride passivation, a Cu/low-k combination offers higher on-chip communication speed and a lower overall device cost. However, the process of packaging Cu/low-k devices has been proven to be difficult, relying either on additional lithography and deposition steps or on costly new process tools. Thus, this paper presents a novel methodology to bond fine pitch Au wire directly onto the Cu/low-k pad structure using the industry standard tool set. A Cu/low-k test vehicle is designed with the required slotted low-k fillings for dual damascene chemical mechanical polishing (CMP) process need. In addition, a thin organic passivation film is developed for coating the exposed Cu/low-k pad temporarily from copper oxidation and to provide a wirebondable surface to form the proper interconnects. A design of experiment is performed to optimize wirebonding parameters [power, time, and ultrasonic gauge (USG) bleed], along with key physical contributors from wafer sawing and die attaching steps that impact the interconnect shear strength and quality. In addition, electrical and optical characterization and surface failure analysis are performed to confirm the feasibility of the technology. Finally, reliability results of the pad structure design and recommendations for further process optimization are presented.

Published in:

Advanced Packaging, IEEE Transactions on  (Volume:27 ,  Issue: 3 )

Date of Publication:

Aug. 2004

Need Help?


IEEE Advancing Technology for Humanity About IEEE Xplore | Contact | Help | Terms of Use | Nondiscrimination Policy | Site Map | Privacy & Opting Out of Cookies

A not-for-profit organization, IEEE is the world's largest professional association for the advancement of technology.
© Copyright 2014 IEEE - All rights reserved. Use of this web site signifies your agreement to the terms and conditions.